Fig.7 Thermal runaway triggered by chemical crosstalk between the cathode and anode[47]: (a) time-resolved XRD patterns of charged cathode material; (b) in situ heat generation and oxygen release at different temperatures of charged cathode materials; (c) at 100~500℃, the mixture of cathode and anode releases virtually no oxygen but has sharp heat generation enhancement; (d) cathode and anode cross chemical reaction process